16µm SLA Wax Printing
High-definition photo-polymer wax pattern printing on automated industrial matrix.
TECHNICAL CASE STUDY DOSSIER
Engineered micro-prong wall thicknesses and wax shrinkage compensation on 18K white gold eternity bands, achieving ±0.03mm dimensional seat tolerances across 7 finger sizes.
PROJECT METROLOGY SNAPSHOT
BUYER BRIEF & CONTEXT
A high-growth North American bridal brand needed to transition their core eternity band assortment from a local boutique bench jeweller to a scalable manufacturing partner capable of consistent diamond calibration.
Consistent 360-degree shared-prong setting with minimal metal visibility, uniform finger comfort bevels, and exact diamond table alignment across ring sizes 4 through 10.
Rhino 3D CAD (.3dm) surface model, diamond layout schematic, and brand hallmark vector files.
Market: United States & Canada Fine Jewellery Retail
Aesthetic Target: Minimalist shared-prong eternity band with maximum light return and seamless prong alignment.
ENGINEERING CHALLENGE
The submitted CAD model was drafted for digital rendering rather than lost-wax vacuum investment casting. Micro-prongs were drawn at 0.38mm thickness, which risked incomplete gold fill during vacuum induction casting, and stone seats lacked the necessary 1.5% volumetric shrink compensation.
PRODUCT SPECIFICATIONS
| PARAMETER / SPECIFICATION GATE | SPECIFICATION VALUE | EVIDENCE MODEL |
|---|---|---|
| Alloy Composition | 18K Nickel-Safe White Gold (75.2% Au, Pd/Ag/Cu balance) | [Measured] |
| Gemstone Specification | Lab-Grown CVD Type IIa, DEF color, VS+ clarity, 1.80mm ±0.02mm | [Measured] |
| Prong Configuration | Shared 4-prong scalloped micro-claw with 0.46mm post-polish diameter | [Measured] |
| Dimensional Tolerance | Ring inner diameter ±0.03mm, band height ±0.04mm | [Measured] |
| Initial Production Run | 420 Units (20 units per size/width combination) | [Measured] |
| Hallmark & Identification | Laser engraved interior: 750 assay, brand wordmark, serial number | [Measured] |
| Surface Finish | Multi-stage magnetic tumbling + hand rouge + 0.5µm rhodium bath | [Measured] |
DESIGN & ENGINEERING EXECUTION
Imported client Rhino file into CAD engineering station. Measured cross-sectional wall thickness using digital caliper checks and identified 14 non-fill risk zones on micro-prongs.
Adjusted prong geometry to 0.52mm raw casting dimension (finishing to 0.46mm post-polish). Increased pavilion seat clearance by 0.12mm to guarantee culet isolation. Added 1.6% scale factor for alloy thermal shrinkage.
Printed prototype wax patterns at 16-micron slice resolution on industrial SLA printers to verify physical ring sizing and diamond seat geometry prior to gold casting.
Fabricated vulcanized silicone master molds with dedicated vacuum channels to ensure bubble-free liquid gold flow across the scalloped perimeter.
SAMPLING & REVISION PROTOCOLS
MANUFACTURING EXECUTION
High-definition photo-polymer wax pattern printing on automated industrial matrix.
Induction melting under argon atmosphere in sealed vacuum pressure chambers.
Each diamond handset under 40x Leica stereo-zoom microscopes by master setters.
Progressive ceramic deburring, hand lapidary rouge buffing, and ultra-dense rhodium electroplating.
QUALITY CONTROL & METROLOGY
See Our Full Quality Process →All 420 production rings underwent a rigorous 4-gate verification process: dimensional metrology, optical stone push testing, alloy assay certification, and final cosmetic inspection under polarized light.
| TEST / INSPECTION GATE | PARAMETER & TOLERANCE | MEASURED RESULT | EVIDENCE MODEL |
|---|---|---|---|
| Alloy Composition (XRF) | Gold karatage ≥ 75.0% Au, 0.00% Ni | Passed: 75.22% Au average across batches | [Measured] |
| Dimensional Caliper Check | Internal ring diameter ±0.05mm | Passed: ±0.024mm standard deviation | [Measured] |
| Stone Security Push Test | Mechanical probe pressure on all claws | Passed: 0 stone shifts across 9,240 diamonds | [Measured] |
| Rhodium Coating Thickness | Minimum 0.40µm electroplate depth | Passed: 0.51µm measured average | [Measured] |
FINAL DELIVERED RESULTS
Delivered complete 420-unit production order on schedule within 18 working days of mold approval. All rings met the North American brand’s stringent quality benchmarks, resulting in zero customer returns for stone loss or sizing variance.
CONTINUATION & REPEAT ORDERS
EVIDENCE GALLERY
Every image documents a verified stage of technical development, tooling, or finished quality assurance.
DEMONSTRATED CAPABILITIES
Repeatable manufacturing workflows and technical capabilities validated during production.
Transformed purely aesthetic digital surface CAD into structurally castable, high-integrity tooling geometry.
Engineered alloy-specific volumetric thermal compensation for 18K white gold.
Maintained stone calibration and seating consistency across high-density pavé layouts.
COMPANION DOSSIERS
START YOUR PROJECT
Share your design, reference or collection direction and we will review the appropriate development and production path.